Product Data Sheet

DuraStar Polymer DS2000, Natural

Application/Uses
  • Toys/Sporting goods
  • Writing instruments
Key Attributes
  • Excellent clarity
  • Excellent flow
  • Fast drying times
  • Good chemical resistance
  • Outstanding impact resistance
  • Quick cycle times
Product Description

Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2000 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing United States Food and Drug Administration (FDA) regulations, Durastar DS2000 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.

This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.
The GREENGUARD INDOOR AIR QUALITY CERTIFIED® Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman Copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products.


Typical Properties
 
 
 
Specific Gravity     D 792  1.2 
Density     ISO 1183  1.19 
Mold Shrinkage   Parallel to Flow, 3.2-mm (0.125-in.) thickness  D 955  0.002-0.006 mm/mm (0.002-0.006 in./in.)
 
Tensile Stress @ Yield     D 638  46 MPa (6700 psi)
Tensile Stress @ Break     D 638  53 MPa (7700 psi)
Elongation @ Yield     D 638  5%
Elongation @ Break     D 638  310%
Flexural Modulus     D 790  1900 MPa (2.75 )
Flexural Yield Strength     D 790  67 MPa (9700 psi)
Rockwell Hardness, R Scale     D 785  105 
Izod Impact Strength, Notched 
  @ 23°C (73°F)
D 256  370 J/m (7 ft·lbf/in.)
  @ -40°C (-40°F)
D 256  60 J/m (1.1 ft·lbf/in.)
Impact Strength, Unnotched 
  @ 23°C (73°F)
D 4812  NB 
  @ -40°C (-40°F)
D 4812  NB 
Impact Resistance (Puncture), Energy @ Max. Load 
  @ 23°C (73°F)
D 3763  45 J (33 ft·lbf)
  @ -40°C (-40°F)
D 3763  48 J (35 ft·lbf)
 
Tensile Stress @ Yield     ISO 527  47 MPa
Tensile Stress @ Break     ISO 527  49 MPa
Elongation @ Yield     ISO 527  4%
Elongation @ Break     ISO 527  210%
Flexural Modulus     ISO 178  1750 MPa
Flexural Strength     ISO 178  64 MPa
Izod Impact Strength, Notched 
  @ 23°C
ISO 180  29.6 
  @ -40°C
ISO 180  6.3 
Impact Resistance (Puncture), Energy @ Max. Load 
  @ 23°C
ISO 6603-2  71 J
  @ -40°C
ISO 6603-2  55 J
 
Deflection Temperature 
  @ 0.455 MPa (66 psi)
D 648  73°C (164°F)
  @ 1.82 MPa (264 psi)
D 648  65°C (149°F)
UL Flammability Classification  d 1.5 mm specimen  UL 94  94HB 
 
Deflection Temperature 
  @ 0.455 MPa (66 psi)
ISO 75  73°C
  @ 1.82 MPa (264 psi)
ISO 75  66°C
 
Haze     D 1003  0.3%
Regular Transmittance     D 1003  89%
Total Transmittance     D 1003  91%
 
Drying Temperature       70°C (160°F)
Drying Time       3 hrs
Processing Melt Temperature       250-290°C (480-550°F)
Mold Temperature       15-30°C (60-80°F)
Comments
Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

26-Jun-2002 9:46:40 AM