Product Data Sheet
Tenite Acetate 105E3V36327 Clear, Trsp
|
|
|
| Product Description |
| Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulosic Acetate 105-27 has a plasticizer level of 27%. |
|
| Typical Properties |
| |
| |
| Plasticizer
|
|
27% |
| Specific Gravity
|
D 792 |
1.28 |
| |
|
| Tensile Stress @ Yield
|
D 638 |
33.1 MPa (4800 psi) |
| Tensile Stress @ Break
|
D 638 |
36.5 MPa (5300 psi) |
| Elongation @ Break
|
D 638 |
25% |
| Flexural Modulus
|
D 790 |
2137 MPa (3.1 ) |
| Flexural Yield Strength
|
D 790 |
54.5 MPa (7900 psi) |
| Rockwell Hardness, R Scale
|
D 785 |
82 |
| Izod Impact Strength, Notched
|
|
|
D 256 |
187 J/m (3.5 ft·lbf/in.) |
|
|
D 256 |
48 J/m (0.9 ft·lbf/in.) |
| |
|
| Deflection Temperature
d |
|
|
D 648 |
73°C (163°F) |
|
|
D 648 |
83°C (181°F) |
| Vicat Softening Temperature
d |
D 1525 |
109°C (228°F) |
| |
|
| Water Absorption, 24 h immersion
|
D 570 |
2.3% |
| Soluble Matter Loss
|
D 570 |
0.3% |
| Weight Loss on Heating
[72 hours @ 80°C (176°F)] |
D 706 |
1.8% |
| |
|
|
|
D 542 |
1.46-1.49 |
| Light Transmission
e |
E 308 |
>90% |
| Haze
e |
D 1003 |
<8.5% |
| Specific Heat
@ 23°C (73°F) |
DSC |
1.26-1.67 kJ/kg·K (0.301-0.399 Btu/lb·°F) |
| Thermal Conductivity
|
C 177 |
0.17-0.33 W/m·K (1.2-2.3 ) |
| Coefficient of Linear Thermal Expansion
|
D 696 |
11- /°C (mm/mm·°C) (6- /°F (in./in.·°F)) |
| Mold Shrinkage
|
D 955 |
0.2-0.6% |
| Dielectric Strength
|
D 149 |
11.8-18.7 kV/mm (300-475 V/mil) |
| Dielectric Constant
1 MHz |
D 150 |
3.3-3.8 |
| Dissipation Factor
1 MHz |
D 150 |
0.01-0.15 |
| Volume Resistivity
|
D 257 |
- ohm·cm |
Characteristics Formula 105 - heat stabilized.
Comments Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.
|
| 27-Jun-2001 3:07:00 PM |