Product Data Sheet

Tenite Butyrate 264A3720013 Clear, Trsp

Application/Uses
  • Toys/Sporting goods
Product Description
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers, or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 264-13 has a plasticizer level of 13%. It meets FDA requirements for certain food-contact applications when supplied in specific FDA color numbers.

Typical Properties
 
 
Plasticizer       13%
Specific Gravity     D 792  1.18 
 
Tensile Stress @ Yield     D 638  29.0 MPa (4200 psi)
Tensile Stress @ Break     D 638  39.3 MPa (5700 psi)
Elongation @ Break     D 638  50%
Flexural Modulus     D 790  1241 MPa (1.80 )
Flexural Yield Strength     D 790  39.3 MPa (5700 psi)
Rockwell Hardness, R Scale     D 785  59 
Izod Impact Strength, Notched 
  @ 23°C (73°F)
D 256  283 J/m (5.3 ft·lbf/in.)
  @ -40°C (-40°F)
D 256  101 J/m (1.9 ft·lbf/in.)
 
Deflection Temperature  d
  @ 1.82 MPa (264 psi)
D 648  69°C (156°F)
  @ 0.455 MPa (66 psi)
D 648  81°C (178°F)
Vicat Softening Temperature  d   D 1525  100°C (212°F)
 
Water Absorption, 24 h immersion     D 570  1.4%
Soluble Matter Loss     D 570  0.1%
Weight Loss on Heating   [72 hours @ 80°C (176°F)]  D 707  0.6%
 
     D 542  1.46-1.49 
Light Transmission  e   E 308  >90%
Haze  e   D 1003  <8.5%
Specific Heat   @ 23°C (73°F)  DSC  1.26-1.67 kJ/kg·K (0.301-0.399 Btu/lb·°F)
Thermal Conductivity     C 177  0.17-0.33 W/m·K (1.2-2.3 )
Coefficient of Linear Thermal Expansion     D 696  11- /°C (mm/mm·°C) (6- /°F (in./in.·°F))
Mold Shrinkage     D 955  0.2-0.6%
Dielectric Strength     D 149  11.8-18.7 kV/mm (300-475 V/mil)
Dielectric Constant   1 MHz  D 150  3.3-3.8 
Dissipation Factor   1 MHz  D 150  0.01-0.15 
Volume Resistivity     D 257  - ohm·cm
Characteristics
Formula 264 - base.

Comments
Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.